Home»Grades > Special Alloy > Waspaloy
WaspaloyApplication:Martensitic special steel
CategoryTypeSteel gradeStandardCountry
Grades Special Alloy WaspaloyUNSUSA

Chemical composition%of the ladle analysis of gradeWaspaloy

C(%)Si(%)Mn(%)Cr(%)Mo(%)Co(%)B(%)Al(%)Ti(%)Other(%)
0.070.10.119.754.45140.0051.43Fe(%) 0.75,Zr 0.04
Waspaloy
Mechanical properties of gradeWaspaloy
Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated ConditionBrinell hardness(HBW)
863(≥)458(≥)421323Solution and Aging,Annealing,Ausaging,Q+T,etc141
Physical properties of gradeWaspaloy
PropertyDensity
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
738(≥)515(≥)443221Solution and Aging,Annealing,Ausaging,Q+T,etc131
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
823739675
WaspaloyRange of products
Product typeProductsDimensionProcessesDeliver Status
Plates/SheetsPlates/Sheets0.08-200mm(T)*W*LForging,hot rolling and cold rollingAnnealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel BarRound Bar,Flat Bar,Square BarΦ8-1200mm*LForging,hot rolling and cold rolling,CastBlack,Rough Turning,Shot Blasting,
Coil/StripSteel Coil/Steel Strip0.03-16.0x1200mmCold-Rolled&Hot-RolledAnnealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/TubesSeamless Pipes/Tubes,Welded Pipes/TubesOD:6-219mm x WT:0.5-20.0mmHot extrusion,Cold Drawn,WeldedAnnealed,Solution and Aging,Q+T,ACID-WASHED
Cross Reference Table(Equivalent Grade)
GradeStandardCountryApplication
WaspaloyUNSUSA
Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 57Ni - 19.5Cr - 13.5Co - 4.2Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted, Annealed
WaspaloyUNSUSA
Nickel Alloy, Corrosion and Heat-Resistant, Welded Tubing 57Ni - 19.5Cr - 13.5Co - 4.2Mo - 2.9Ti - 1.4Al - 0.006B - 0.08Zr Consumable Electrode Remelted or Vacuum Induction Melted, Annealed
WaspaloyUNSUSA
Nickel Alloy, Corrosion and Heat-Resistant, Forgings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825 to 1900°F (996 to 1038°C) Solution, Stabilization, and Precipitation Heat Treated
WaspaloyUNSUSA
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900°F Solution Heat Treated
WaspaloyUNSUSA
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode Remelted or Vacuum Induction Melted 1825 to 1900°F (996 to 1038°C) Solution, Stabilization, and Pre
WaspaloyUNSUSA
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Wire Forgings, and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975°F (1079°C) Solution Heat Treated
WaspaloyUNSUSA
Nickel Alloy, Corrosion and Heat-Resistant, Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975°F (1079°C) Solution, Stabilization, and Precipitation Heat Treated
WaspaloyUNSUSA
Nickel Alloy, Corrosion and Heat Resistant, Welding Wire 57Ni - 19.5Cr - 13.5Co - 4.2Mo - 3.1Ti - 1.4Al - 0.006B Vacuum Induction Melted, Solution Heat Treated
WaspaloyUNSUSA
Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 57Ni - 19.5Cr - 13.5Co - 4.2Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted, Annealed
WaspaloyUNSUSA
Nickel Alloy, Corrosion and Heat-Resistant, Welded Tubing 57Ni - 19.5Cr - 13.5Co - 4.2Mo - 2.9Ti - 1.4Al - 0.006B - 0.08Zr Consumable Electrode Remelted or Vacuum Induction Melted, Annealed
WaspaloyUNSUSA
Nickel Alloy, Corrosion and Heat-Resistant, Forgings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825 to 1900°F (996 to 1038°C) Solution, Stabilization, and Precipitation Heat Treated
WaspaloyUNSUSA
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900°F Solution Heat Treated
WaspaloyUNSUSA
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode Remelted or Vacuum Induction Melted 1825 to 1900°F (996 to 1038°C) Solution, Stabilization, and Pre
WaspaloyUNSUSA
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Wire Forgings, and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1975°F (1079°C) Solution Heat Treated
WaspaloyUNSUSA
Nickel Alloy, Corrosion and Heat-Resistant, Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975°F (1079°C) Solution, Stabilization, and Precipitation Heat Treated
WaspaloyUNSUSA
Nickel Alloy, Corrosion and Heat Resistant, Welding Wire 57Ni - 19.5Cr - 13.5Co - 4.2Mo - 3.1Ti - 1.4Al - 0.006B Vacuum Induction Melted, Solution Heat Treated
WaspaloyUNSUSA
Special Purpose Alloys ("Superalloys")
WaspaloyUNSUSA
Engine poppet valve information report

Relevant products

Enquiry