Home»Grades > Special Alloy > 317S17
317S17Application:austenitic special steel
CategoryTypeSteel gradeCountry
Grades Special Alloy 317S17UK

Chemical composition%of the ladle analysis of grade317S17

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Ni(%)Mo(%)
Max 0.08Max 1.00Max 1.00Max 0.045Max 0.0318.0-20.012.0-15.03.00-4.00
317S17
Mechanical properties of grade317S17
Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated ConditionBrinell hardness(HBW)
647(≥)575(≥)422234Solution and Aging,Annealing,Ausaging,Q+T,etc134
Physical properties of grade317S17
PropertyDensity
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
612(≥)153(≥)241324Solution and Aging,Annealing,Ausaging,Q+T,etc121
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
641618751
317S17Range of products
Product typeProductsDimensionProcessesDeliver Status
Plates/SheetsPlates/Sheets0.08-200mm(T)*W*LForging,hot rolling and cold rollingAnnealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel BarRound Bar,Flat Bar,Square BarΦ8-1200mm*LForging,hot rolling and cold rolling,CastBlack,Rough Turning,Shot Blasting,
Coil/StripSteel Coil/Steel Strip0.03-16.0x1200mmCold-Rolled&Hot-RolledAnnealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/TubesSeamless Pipes/Tubes,Welded Pipes/TubesOD:6-219mm x WT:0.5-20.0mmHot extrusion,Cold Drawn,WeldedAnnealed,Solution and Aging,Q+T,ACID-WASHED
Cross Reference Table(Equivalent Grade)
GradeStandardCountryApplication
317S17UK
Specification for stainless and heat-resisting steel round wire

Enquiry