CNS CNS 304N2Enquiry|Print this page
Category | Type | Steel grade | Standard | Country |
---|---|---|---|---|
Grades | Special Alloy | CNS 304N2 | CNS | China |
Chemical composition%of the ladle analysis of gradeCNS 304N2
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | N(%) | Nb(%) |
---|---|---|---|---|---|---|---|---|
Max 0.08 | Max 1.00 | Max 2.50 | Max 0.045 | Max 0.030 | 18.00-20.00 | 7.50-10.50 | 0.15-0.30 | Max 0.15 |
Proof strength Rp0.2(MPa) | Tensile strength Rm(MPa) | Impact energy KV(J) | Elongation at fracture A(%) | Reduction in cross section on fracture Z(%) | As-Heat-Treated Condition | Brinell hardness(HBW) |
---|---|---|---|---|---|---|
326(≥) | 558(≥) | 24 | 44 | 34 | Solution and Aging,Annealing,Ausaging,Q+T,etc | 444 |
Property | Density kg/dm3 | Temperature T °C/F | Specific heat J/kgK | Thermal conductivity W/mK | Electric resistance µΩ·cm | Modulus of elasticity kN/mm2 | Expansion rate |
---|---|---|---|---|---|---|---|
363(≥) | 541(≥) | 21 | 14 | 13 | Solution and Aging,Annealing,Ausaging,Q+T,etc | 221 | |
Temp. °C/°F | Creep strain limit (10000h) (Rp1,0)N/mm2 | Creep rupture strength (10000h) (Rp1,0)N/mm2 | |||||
764 | 236 | 992 |
Product type | Products | Dimension | Processes | Deliver Status |
---|---|---|---|---|
Plates/Sheets | Plates/Sheets | 0.08-200mm(T)*W*L | Forging,hot rolling and cold rolling | Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting |
Steel Bar | Round Bar,Flat Bar,Square Bar | Φ8-1200mm*L | Forging,hot rolling and cold rolling,Cast | Black,Rough Turning,Shot Blasting, |
Coil/Strip | Steel Coil/Steel Strip | 0.03-16.0x1200mm | Cold-Rolled&Hot-Rolled | Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting |
Pipes/Tubes | Seamless Pipes/Tubes,Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion,Cold Drawn,Welded | Annealed,Solution and Aging,Q+T,ACID-WASHED |
Grade | Standard | Country | Application |
---|---|---|---|
STS304N2 | CNS | China | Stainless steel bars |
304N2 | CNS | China | Stainless steel bars |